Used in dryers in gas phase, liquid phase and auto-instrument wind drying of petrochemical, textile and oxygen-making industries, PSA in air-separation etc. Due to high heat-adsorption quantity of single molecular adsorbing layer, so it is very suitable for the use of heat-free regeneration device.
Type & Size | Bulk density g/cm3 | Specific Surface m2/g | Pore volume cm3/g | Static adsorption adsorption % (RH=60%) | Crushing trength N/sphere | Initial abrasion rate % | |
---|---|---|---|---|---|---|---|
AG-A1 | φ3-5 | ≥ 0.70 | ≥ 280 | ≥ 0.38 | ≥ 15.2 | ≥ 70 | ≤ 0.40 |
AG-A2 | φ3-5 | ≥ 0.70 | ≥ 300 | ≥ 0.40 | ≥ 17.3 | ≥ 80 | ≤ 0.40 |
φ4-6 | ≥ 0.68 | ≥ 300 | ≥ 0.40 | ≥ 17.3 | ≥ 120 | ≤ 0.40 | |
φ5-7 | ≥ 0.70 | ≥ 300 | ≥ 0.40 | ≥ 17.3 | ≥ 130 | ≤ 0.40 | |
φ6-8 | ≥ 0.68 | ≥ 300 | ≥ 0.40 | ≥ 16.4 | ≥ 130 | ≤ 0.40 | |
AG-A3 | φ3-5 | ≥ 0.68 | ≥ 300 | ≥ 0.40 | ≥ 17.3 | ≥ 80 | ≤ 0.60 |
φ4-6 | ≥ 0.68 | ≥ 300 | ≥ 0.40 | ≥ 17.2 | ≥ 110 | ≤ 0.60 | |
φ5-7 | ≥ 0.68 | ≥ 300 | ≥ 0.42 | ≥ 17.5 | ≥ 120 | ≤ 0.80 | |
φ6-8 | ≥ 0.68 | ≥ 300 | ≥ 0.42 | ≥ 16.3 | ≥ 120 | ≤ 0.80 | |
AG-A4 | φ3-5 | ≥ 0.68 | ≥ 350 | ≥ 0.45 | ≥ 19.2 | ≥ 80 | ≤ 0.40 |
φ4-6 | ≥ 0.68 | ≥ 350 | ≥ 0.45 | ≥ 19.4 | ≥ 110 | ≤ 0.60 | |
φ5-7 | ≥ 0.68 | ≥ 350 | ≥ 0.45 | ≥ 19.4 | ≥ 110 | ≤ 0.60 |
Packing | : | 25 Kgs triple layer paper PP bag/25 kgs. HDPE drum/125 kgs. Galvanized air-tight steel drum with Linen sealed |